Iron-based High-strength Metal Injection Molded Parts
1720079803600_1.jpg_w720
1720079803600_2.png_w720
1720079803600_3.png_w720
1720079803600_4.png_w720
1/2
<< /span>
>

Hlau - raws qhov siab - muaj zog molding qhov chaw

Mim yog cov lus luv ntawm cov hlau txhaj tshuaj. Hlau hmoov txhaj tshuaj molding tshuab yog cov khoom ntawm kev nkag mus thiab kev sib tshuam xws li cov tshuaj siv yas yas, cov hmoov me me me thiab cov khoom siv hlau mould.

Mim yog cov lus luv ntawm cov hlau txhaj tshuaj. Hlau hmoov txhaj tshuaj molding tshuab yog cov khoom ntawm kev nkag mus thiab kev sib tshuam xws li cov tshuaj siv yas yas, cov hmoov me me me thiab cov khoom siv hlau mould.

 

Qhov zoo ntawm MIM MIM sib xyaw ua ke ntawm hmoov metallurgy thiab kev txhaj tshuaj yas moulding, thiab siv cov khoom siv yas ua kom zoo nkauj thiab siv cov khoom siv. Nws tau dhau los ua ib tug nyob ze- Cov khoom siv thev naus laus zis rau kev tsim khoom zoo niaj hnub, cov hmoov tsis txaus ntseeg ntawm cov hmoov uas tsis muaj zog, machining thiab precision casting.

 

Piv nrog rau lwm cov txheej txheem hlau tsim xws li cov hlau ntawv hlau ua, hmoov moulding, hmoov moulding, forging thiab machining tuaj yeem tsim cov duab geometric.

 

Feem ntau hais lus, Mim tseem tuaj yeem ua tiav cov qauv hauv cov nyom uas tuaj yeem ua tiav los ntawm kev txhaj tshuaj yas molding.

 

Ua ntawv thov cov yeeb yaj kiab no, MIM muaj lub sijhawm los sib koom ua ke ntau ntu los ntawm lwm cov khoom siv hlau, txo cov khoom lag luam kom txo cov khoom siv sib dhos ntawm cov khoom.

 

Cov khoom siv peev txheej siab mim moulding yog ib nyob ze - roj molding txheej txheem. Cov duab ntawm nws qhov chaw yog ze rau daim ntawv foos kawg, thiab cov khoom siv cov nyiaj siv tau yog qhov siab, uas yog qhov tshwj xeeb rau kev ua kom muaj cov khoom ploj.

 

Lub microstructure ntawm feem yog cov khaub ncaws hnav zoo, lub ntom yog qhov siab, thiab kev ua tau zoo. Mim yog cov txheej txheem tshuaj moulding. Lub xub ntiag ntawm cov nplaum ua kom cov txheej txheem sib txawv ntawm cov hmoov, thiab tom qab ntawd cov khoom ntom ntawm cov khoom lag luam sintered tuaj yeem ncav cuag txoj kev xav ntawm nws cov khoom.

 

Feem ntau hais lus, MIM tuaj yeem ncav cuag 95% ~ 99% ntawm theoretical density. Kev ntom ntom siab tuaj yeem ua rau lub zog ntawm cov mim ntu, txhim kho kev sib zog thiab hluav taws xob thiab thermal cov khoom sib nqus.

Qhov ceev ntawm cov seem tau nias cov hmoov ua hmoov moulding tsuas tuaj yeem ncav cuag 85% ntawm theoretical ceev ntawm feem ntau. Qhov no yog feem ntau yog vim kev sib txhuam ntawm cov pwm ntsa thiab cov hmoov thiab ntawm cov hmoov, uas ua rau qhov tsis sib xws me me ntawm cov nias. Qhov no yuav ua rau cov nias cov hmoov metallurgy kom txo cov txiaj ntsig no, yog li cov khoom siv tsis zoo, thiab cov khoom siv tsis zoo, thiab cov khoom siv tsis zoo, uas tsis cuam tshuam rau cov khoom siv hluav taws xob, uas muaj feem xyuam rau cov khoom siv hauv cov tshuab.

 

High efficiency, yooj yim kom ua tiav loj- nplai thiab loj} Kev tsim kev txhaj tshuaj molding tshuab, uas tsim nyog rau loj- nplai noj; Nyob rau tib lub sijhawm, qhov sib xws ntawm kev txhaj tshuaj molding cov khoom yog qhov zoo, uas muab kev lees paub rau kev noj khoom haus loj thiab loj} nplai kev noj.

 

Kev siv ntau yam ntawm cov ntaub ntawv tsim nyog thiab cov ntaub ntawv dav hlau cov ntaub ntawv tsim rau Mim muaj ntau heev. Hauv cov ntsiab lus, cov khoom siv hmoov uas tuaj yeem muab pov rau qhov kub thiab cov txheej txheem nyuaj, suav nrog cov ntaub ntawv nyuaj, suav nrog cov ntaub ntawv me me hauv cov txheej txheem kev lag luam ib txwm muaj. Cov ntaub ntawv hlau uas tuaj yeem ua tiav los ntawm Mim suav nrog cov hlau qis, titanium alloy, sivar ecoy, cemar, kev sib nqus, cov lus sib nqus, thiab lwm yam.

 

Ib qho ntxiv, MIM kuj tseem tuaj yeem ua cov ntaub ntawv siv mis ua raws li cov neeg siv khoom, tsim cov ntaub ntawv aluminium, thiab tsim cov khoom sib xyaw ua ke rau hauv ntu.

 

Mim molding ntawm tsis {{0} ferrorous alloy aluminium thiab nws feem ntau yog txheej txheem los ntawm lwm cov qauv kev lag luam ntau dua, xws li tuag casting lossis machining.

 

Qinhuangdao Zhongwei Precision Machinery Co., Ltd. specializes in the production of powder metallurgy products such as high-precision, low-noise oil-containing bearings and high-performance mechanical structural parts. Kev Txhaj Tshuaj Moulding faib (MIM) tshwj xeeb hauv kev tsim cov complex, siab} precision yam nrog kev tiv thaiv kev nplua nuj thiab kev tiv thaiv ib puag ncig. Lub tuam txhab cov khoom tseem ceeb suav nrog Copper-}}}}}}} - zoo li cov txheej txheem zoo li cov txheej txheem. Siv dav hauv cov khoom siv hauv yim neeg, cov cuab yeej siv hluav taws xob, chaw ua haujlwm, xauv kev lag luam, kev lag luam khoom muag thiab lwm yam lag luam.

 

Qinhuangdao Zhongwe lub prefision Machinery Co., Ltd. Lub tuam txhab nyob hauv Qinhuangdao siab {{} Tech thaj chaw, nrog cov kev daws teeb meem R & D thiab cov khoom siv tau zoo thiab ua haujlwm ruaj khov.

 

Txij li thaum nws tsim tau, lub tuam txhab tau ib txwm ua raws li cov ntsiab cai ntawm cov qhua tuaj noj mov {{}-} ua ntej, kev txhim kho ywj siab thiab txhim kho tshiab. Thev naus laus zis - thawj txoj cai txhim kho.

 

Lub tuam txhab ua lag luam tseem ceeb yog kev tshawb fawb thiab kev tsim kho, tsim qauv, ntau lawm thiab muag khoom ntawm cov qauv hlau khoom. Cov khoom tuaj yeem siv dav hauv cov ntawv thov tseem ceeb xws li cov khoom siv hluav taws xob cov khoom siv, khoom siv kho mob, thiab tsheb. Nws muaj qhov zoo thiab kev muaj kev nplua nuj nyob hauv kev tshawb fawb thiab kev txhim kho, cov qauv tsim, tsim cov khoom lag luam, thiab lwm yam.

 

Lub tuam txhab muaj pab pawg tseem ceeb, cov cuab yeej ua tau zoo heev, thiab tau tshaj tawm cov khoom siv cov cim kev sib tw thiab ua tus khub zoo nkauj rau cov neeg siv khoom hauv ntiaj teb.

 

Xa kev nug

(0/10)

clearall